J. Turbomach. October 2007, 129(4): 791–799.
Published Online: September 5, 2006
... the effective thermal properties and the permeability of these multilayer plates, a multiscale approach based on the homogenization technique is employed. This method allows the calculation of effective equivalent properties either for each layer or for the multilayer of superalloy, bondcoat, and thermal...