The paper describes some experimental work designed to investigate the bursting of pipe and pressure vessels by gaseous detonation. The test specimens were 3.25-in-OD tubes, 12 in. long, and of 0.040 to 0.070-in. wall thickness. The specimens, cut from hot-rolled carbon-steel pipe, and also from drawn carbon-steel tubing, were tested at several temperatures, which were chosen to produce failures both above and below the brittle transition temperatures for the two materials. In addition, an austenitic stainless-steel specimen was tested under very severe conditions in several unsuccessful attempts to fragment it.
Issue Section:
Research Papers
This content is only available via PDF.
Copyright © 1961
by ASME